Inch Square Washer Steel
d | a | h |
---|---|---|
1.1/2” | 5/16” | 1/8” |
1.1/2” | 3/8” | 1/8” |
2” | 3/8” | 1/8” |
3” | 3/8” | 1/8” |
1.1/2” | 1/2” | 1/8” |
2” | 1/2” | 1/8” |
2.1/2” | 1/2” | 1/8” |
3” | 1/2” | 1/8” |
1.1/2” | 5/8” | 1/8” |
2” | 5/8” | 1/8” |
3” | 5/8” | 1/8” |
2” | 3/4” | 1/8” |
3” | 3/4” | 1/8” |
2” | 1/2” | 1/4” |
3” | 1/2” | 1/4” |
4” | 1/2” | 1/4” |
3” | 5/8” | 1/4” |
4” | 5/8” | 1/4” |
3” | 3/4” | 1/4” |
3” | 1” | 1/4” |
4” | 1” | 1/4” |
Weight | 0.0000 |
---|---|
Material | STEEL |
Standard Number | . |
Second Standard | - |
Drive | Non |
Head | NON |
American Generic Brand Term | - |
Diameter | 1.1/2”,2”,3”,2.1/2”,4” |
Length | NON |