Inch Square Washer Steel
| d | a | h |
|---|---|---|
| 1.1/2” | 5/16” | 1/8” |
| 1.1/2” | 3/8” | 1/8” |
| 2” | 3/8” | 1/8” |
| 3” | 3/8” | 1/8” |
| 1.1/2” | 1/2” | 1/8” |
| 2” | 1/2” | 1/8” |
| 2.1/2” | 1/2” | 1/8” |
| 3” | 1/2” | 1/8” |
| 1.1/2” | 5/8” | 1/8” |
| 2” | 5/8” | 1/8” |
| 3” | 5/8” | 1/8” |
| 2” | 3/4” | 1/8” |
| 3” | 3/4” | 1/8” |
| 2” | 1/2” | 1/4” |
| 3” | 1/2” | 1/4” |
| 4” | 1/2” | 1/4” |
| 3” | 5/8” | 1/4” |
| 4” | 5/8” | 1/4” |
| 3” | 3/4” | 1/4” |
| 3” | 1” | 1/4” |
| 4” | 1” | 1/4” |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | . |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | - |
| Diameter | 1.1/2”,2”,3”,2.1/2”,4” |
| Length | NON |