Metric Double Coil Rectangular Section Spring Washer Spring-Steel BS4464
Metric Double Coil Rectangular Section Spring Washer Spring-Steel BS4464
Metric Double Coil Rectangular Section Spring Washer Spring-Steel BS4464 d/c rect split lock washer BS 4464
s
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | DIN127 |
| Second Standard | BS4464 |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | THANKERY,SPLITLOCK |
| Diameter | M5,M6,M8,M10,M12,M14,M16,M18,M20,M22,M24 |
| Length | NON |