Inch BA Rectangular Section Spring Washer Spring-Steel BS1802B
Inch BA Rectangular Section Spring Washer Spring-Steel BS1802B
| D | d1 max | d1 min | d2 max | s1 | swg | s | swg |
|---|---|---|---|---|---|---|---|
| 6BA | 0.1370 | 0.1290 | 0.2370 | 0.0480 | 18.0000 | 0.0320 | 21.0000 |
| 4BA | 0.1700 | 0.1600 | 0.3000 | 0.0640 | 16.0000 | 0.0320 | 21.0000 |
| 2BA | 0.2020 | 0.1920 | 0.3870 | 0.0920 | 13.0000 | 0.0480 | 18.0000 |
Inch BA Rectangular Section Spring Washer Spring-Steel BS 1802 B
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | BS1802B |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | SPLITLOCK |
| Diameter | 2BA,4BA,6BA |
| Length | NON |