Inch Internal Toothed Heavy Shakeproof Washer Spring-Steel B18.21.1T7

SKU: 1461
Details
Details

Inch Internal Toothed Heavy Shakeproof Washer Spring-Steel B18.21.1T7

 

SizeSizeA MaxA MinB MaxB MinC MaxC Min
1/4" 0.2500 0.2670 0.2560 0.5360 0.5000 0.0450 0.0350
5/16" 0.3125 0.3320 0.3200 0.6070 0.5900 0.0500 0.0400
3/8" 0.3750 0.3980 0.3840 0.7480 0.7000 0.0500 0.0420
7/16" 0.4375 0.4640 0.4480 0.8580 0.8000 0.0670 0.0500
1/2" 0.5000 0.5300 0.5120 0.9240 0.8800 0.0670 0.0550
9/16" 0.5625 0.5960 0.5760 1.0340 0.9900 0.0670 0.0550
5/8" 0.6250 0.6630 0.6400 1.1350 1.1000 0.0670 0.0590
3/4" 0.7500 0.7950 0.7680 1.2650 1.2400 0.0840 0.0700
7/8" 0.8750 0.9270 0.8940 1.4470 1.4000 0.0840 0.0750
Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberB18.2.1.1T7
Second Standard-
DriveNon
HeadNON
American Generic Brand TermLOCKWASHER
Diameter0
LengthNON