SizeSizeA MaxA MinB MaxB MinC Max C Min
No.30.09900.10900.10200.23500.22000.01600.0100
No.40.11200.12300.11500.26000.24500.01800.0120
No.50.12500.13600.12900.28500.27000.02000.0140
No.60.13800.15000.14100.32000.30500.02200.0160
No.80.16400.17600.16800.38100.36500.02300.0180
No.100.19000.20400.19500.41000.39500.02400.0180
No.120.21600.23100.22100.47500.46000.02700.0200
1/4"0.25000.26700.25600.51000.49400.02800.0230
5/16"0.31250.33200.03200.61000.58800.03400.0280
3/8"0.37500.39800.38400.69400.67000.04000.0320
7/16"0.43750.46400.44800.76000.74000.04000.0320
1/2"0.50000.53000.51300.90000.88000.04500.0370
9/16"0.56250.59600.57600.98500.96000.04500.0370
5/8"0.62500.66300.64101.07001.04500.05000.0420
11/16"0.68750.72800.70401.15501.13000.05000.0420
3/4"0.75000.79500.76801.26001.22000.05500.0470
13/16"0.81250.86100.83301.31501.29000.05500.0470
7/8"0.87500.92700.89701.41001.38000.06000.0520
1"1.00001.06021.02501.62001.59000.06700.0590
Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberB18.21.1T8
Second Standard-
DriveNon
HeadNON
American Generic Brand TermLOCKWASHER
Diameter0
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.