Metric Conical Seat Washer Stainless-Steel-A4 DIN6319D
SKU:
1568
Details
Details
Metric Conical Seat Washer Stainless-Steel-A4 DIN6319D
| D | d2 | d3 | h2 |
|---|
| M6 | 7.1000 | 12.0000 | 2.8000 |
| M8 | 9.0000 | 17.0000 | 3.5000 |
| ?10 | 12.0000 | 21.0000 | 4.2000 |
| M12 | 14.2000 | 24.0000 | 5.0000 |
| M14 | 16.5000 | 28.0000 | 5.6000 |
| M16 | 19.0000 | 30.0000 | 6.2000 |
| M20 | 23.2000 | 36.0000 | 7.5000 |
| M24 | 28.0000 | 44.0000 | 9.5000 |
| M30 | 35.0000 | 56.0000 | 12.0000 |
| M36 | 42.0000 | 68.0000 | 15.0000 |
| M42 | 49.0000 | 78.0000 | 18.0000 |
| M48 | 56.0000 | 92.0000 | 22.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A4 |
|---|
| Standard Number | DIN6319D |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M6,M8,?10,M12,M14,M16,M20,M24 |
|---|
| Length | NON |
|---|