dlegsBC thicknesspush on force kgpull off force kg
1/16"40.3820.0084kg20kg
3/32"40.3820.0085kg20kg
1/8"40.3820.00812kg20kg
5/32"50.4520.0087kg40kg
3/16"60.4520.0086kg40kg
7/32"60.4520.00813kg40kg
1/4"60.6020.01011kg80kg
9/32"60.6020.01020kg80kg
5/16"60.6020.01022kg80kg
11/32"60.7260.01217kg100kg
3/8"60.7260.01221kg100kg
7/16"60.9850.01615kg250kg
1/2"60.9850.01635kg250kg
5/8"60.9850.01661kg250kg
3/4"91.4400.01616kg350kg
7/8"91.5000.01846kg350kg
1"91.6290.02072kg385kg