dd1 mind1 maxd2 maxd2 minh nomh maxh min
2.21.90002.00005.00004.82001.00001.06000.9400
2.92.50002.60007.00006.64001.00001.06000.9400
3.53.00003.10008.00007.64001.00001.06000.9400
4.23.55003.67009.00008.64001.00001.06000.9400
4.84.00004.120010.00009.64001.00001.06000.9400
5.54.70004.820012.000011.57001.60001.06001.5200
6.35.40005.520014.000013.57001.60001.68001.5200
87.15007.300016.000015.57001.60001.68001.5200
9.58.80008.950020.000019.48002.00002.09001.9100