Metric Flat Washer For Sems Self Tapping Screws Type L Steel-200Hv ISO10644

SKU: 2300
Details
Details
Metric Flat Washer For Sems Self Tapping Screws Type L Steel-200Hv ISO10644
dd1 mind1 maxd2 maxd2 minh nomh maxh min
2.21.90002.00007.00006.64001.00001.60000.9400
2.92.50002.60009.00008.64001.00001.60000.9400
3.53.00003.100011.00001.57001.00001.60000.9400
4.23.55003.670012.000011.57001.00001.60000.9400
4.84.00004.120015.000014.57001.60001.68001.5200
5.54.70004.820015.000014.57001.60001.68001.5200
6.35.40005.520018.000017.57001.60001.68001.5200
87.15007.300024.000023.48002.00002.90001.9100
9.58.80008.95003.000029.48002.50002.59002.4100
Additional Info
Additional Info
Weight0.0000
MaterialSteel-200Hv
Standard NumberISO10644
Second Standard-
DriveNon
HeadNON
American Generic Brand TermSEMS
Diameter 2.20,2.90,3.50,4.20,4.80,5.50,6.30,8.00,9.50