Metric Countersunk Washer Steel

 d1  d2  d3  s 
           4        10     8.40     2.50
           4        13     8.40     2.50
           5        13  10.50     3.00
           5        16  10.50     3.00
           6        15  12.60     4.00
           6        20  12.60     4.00
           8        20  16.80     5.00
           8        26  16.80     5.00
        10        25  21.00     6.50
        10        32  21.00     6.50
        12        30  25.20     7.50
        12        40  25.20     7.50  fastenerdata



 

 

Metric Countersunk Washer Steel

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL