Metric Coarse Captive Washer For DIN7964 Items Stainless-Steel-A2
| d | d1 min | d2 | s | b max | c min |
|---|
| M4 | 4.1000 | 19.5000 | 0.4000 | 3.8000 | 2.7000 |
| M5 | 5.1000 | 20.5000 | 0.5000 | 4.0000 | 2.7000 |
| M6 | 6.1000 | 21.5000 | 0.6000 | 4.2000 | 2.7000 |
| M8 | 8.1000 | 25.0000 | 0.8000 | 5.4000 | 2.7000 |
| M10 | 10.1000 | 27.5000 | 1.0000 | 5.8000 | 2.7000 |
| M12 | 12.1000 | 29.5000 | 1.2000 | 6.5000 | 2.7000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A2 |
|---|
| Standard Number | . |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | WAISTED |
|---|
| Diameter | M4,M5,M6,M8,M10,M12,M14,M16 |
|---|
| Length | NON |
|---|