Metric Electrical Connection Oval Washer Steel DIN46288A

SKU: 2428
Details
Details

Metric Electrical Connection Oval Washer Steel DIN46288A DIN 46288


dd1 mind1 maxa mina maxb minb maxs mins maxh minh max
M33.20003.50005.90006.10006.85007.15001.10001.30002.40002.6000
M3.53.70004.00006.90007.10008.35008.65001.36001.44002.90003.1000
M55.30005.600011.300011.700012.800013.20001.60001.80004.10004.3000
M55.30005.600011.300011.700013.800014.20001.60001.80004.10004.3000
M66.40006.800014.500015.000016.000016.50002.00002.25005.50005.8000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN46288A
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter M3,M3.5,M5,M6