Metric Protection Washer Stainless-Steel-A4 DIN7349
SKU:
1337
Details
Details
Metric Protection Washer Stainless-Steel-A4 DIN7349
| D | d1 | h | d2 |
|---|
| M3 | 3.2000 | 1.0000 | 9.0000 |
| M4 | 4.3000 | 1.6000 | 12.0000 |
| M5 | 5.3000 | 2.0000 | 15.0000 |
| M6 | 6.4000 | 3.0000 | 17.0000 |
| M8 | 8.4000 | 4.0000 | 21.0000 |
| M10 | 10.5000 | 4.0000 | 25.0000 |
| M12 | 13.0000 | 6.0000 | 30.0000 |
| M14 | 15.0000 | 6.0000 | 36.0000 |
| M16 | 17.0000 | 6.0000 | 40.0000 |
| M20 | 21.0000 | 8.0000 | 44.0000 |
| M22 | 23.0000 | 8.0000 | 50.0000 |
| M24 | 25.0000 | 10.0000 | 50.0000 |
| M30 | 31.0000 | 10.0000 | 68.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A4 |
|---|
| Standard Number | DIN7349 |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M3,M4,M5,M6,M8,M10,M12,M14,M16,M20,M22,M24,M30 |
|---|
| Length | NON |
|---|