Schnorr Metric Conical Disc Springs Spring-Steel DIN2093 35.5 to 90mm
| De | Di | t | t' | lo | ho | ho/t | ho’/t’ | Article |
| 35.5 | 18.30 | 0.90 | 2.05 | 1.15 | 1.28 | 011850C | ||
| 35.5 | 18.30 | 1.25 | 2.25 | 1.00 | 0.80 | 011900B | ||
| 35.5 | 18.30 | 2.00 | 2.80 | 0.80 | 0.40 | 012000A | ||
| 40 | 14.30 | 1.25 | 2.65 | 1.40 | 1.12 | 12100 | ||
| 40 | 14.30 | 1.50 | 2.75 | 1.25 | 0.83 | 12200 | ||
| 40 | 14.30 | 2.00 | 3.05 | 1.05 | 0.53 | 12300 | ||
| 40 | 16.30 | 1.50 | 2.80 | 1.30 | 0.87 | 12400 | ||
| 40 | 16.30 | 2.00 | 3.10 | 1.10 | 0.55 | 12500 | ||
| 40 | 18.30 | 2.00 | 3.15 | 1.15 | 0.58 | 12600 | ||
| 40 | 20.40 | 1.00 | 2.30 | 1.30 | 1.30 | 012700C | ||
| 40 | 20.40 | 1.50 | 2.65 | 1.15 | 0.77 | 012800B | ||
| 40 | 20.40 | 2.00 | 3.10 | 1.10 | 0.55 | 12900 | ||
| 40 | 20.40 | 2.25 | 3.15 | 0.90 | 0.40 | 013000A | ||
| 40 | 20.40 | 2.50 | 3.45 | 0.95 | 0.38 | 13100 | ||
| 45 | 22.40 | 1.25 | 2.85 | 1.60 | 1.28 | 013250C | ||
| 45 | 22.40 | 1.75 | 3.05 | 1.30 | 0.74 | 013300B | ||
| 45 | 22.40 | 2.50 | 3.50 | 1.00 | 0.40 | 013400A | ||
| 50 | 18.40 | 1.25 | 2.85 | 1.60 | 1.28 | 13500 | ||
| 50 | 18.40 | 1.50 | 3.30 | 1.80 | 1.20 | 13600 | ||
| 50 | 18.40 | 2.00 | 3.50 | 1.50 | 0.75 | 13700 | ||
| 50 | 18.40 | 2.50 | 4.10 | 1.60 | 0.64 | 13800 | ||
| 50 | 18.40 | 3.00 | 4.40 | 1.40 | 0.47 | 13900 | ||
| 50 | 20.40 | 2.00 | 3.50 | 1.50 | 0.75 | 14000 | ||
| 50 | 20.40 | 2.50 | 3.85 | 1.35 | 0.54 | 14100 | ||
| 50 | 22.40 | 2.00 | 3.60 | 1.60 | 0.80 | 14200 | ||
| 50 | 22.40 | 2.50 | 3.90 | 1.40 | 0.56 | 14300 | ||
| 50 | 25.40 | 1.25 | 2.85 | 1.60 | 1.28 | 014400C | ||
| 50 | 25.40 | 1.50 | 3.10 | 1.60 | 1.07 | 14500 | ||
| 50 | 25.40 | 2.00 | 3.40 | 1.40 | 0.70 | 014600B | ||
| 50 | 25.40 | 2.50 | 3.90 | 1.40 | 0.56 | 14700 | ||
| 50 | 25.40 | 3.00 | 4.10 | 1.10 | 0.37 | 014800A | ||
| 56 | 28.50 | 1.50 | 3.45 | 1.95 | 1.30 | 014950C | ||
| 56 | 28.50 | 2.00 | 3.60 | 1.60 | 0.80 | 015000B | ||
| 56 | 28.50 | 3.00 | 4.30 | 1.30 | 0.43 | 015100A | ||
| 60 | 20.50 | 2.00 | 4.10 | 2.10 | 1.05 | 15200 | ||
| 60 | 20.50 | 2.50 | 4.30 | 1.80 | 0.72 | 15300 | ||
| 60 | 20.50 | 3.00 | 4.70 | 1.70 | 0.57 | 15400 | ||
| 60 | 25.50 | 2.50 | 4.40 | 1.90 | 0.76 | 15500 | ||
| 60 | 25.50 | 3.00 | 4.65 | 1.65 | 0.55 | 15600 | ||
| 60 | 30.50 | 2.50 | 4.30 | 1.80 | 0.72 | 15700 | ||
| 60 | 30.50 | 3.00 | 4.70 | 1.70 | 0.57 | 15800 | ||
| 60 | 30.50 | 3.50 | 5.00 | 1.50 | 0.43 | 15900 | ||
| 63 | 31.00 | 1.80 | 4.15 | 2.35 | 1.31 | 016050C | ||
| 63 | 31.00 | 2.50 | 4.25 | 1.75 | 0.70 | 016100B | ||
| 63 | 31.00 | 3.00 | 4.80 | 1.80 | 0.60 | 16200 | ||
| 63 | 31.00 | 3.50 | 4.90 | 1.40 | 0.40 | 016300A | ||
| 70 | 25.50 | 2.00 | 4.50 | 2.50 | 1.25 | 16400 | ||
| 70 | 30.50 | 2.50 | 4.90 | 2.40 | 0.96 | 16500 | ||
| 70 | 30.50 | 3.00 | 5.10 | 2.10 | 0.70 | 16600 | ||
| 70 | 35.50 | 3.00 | 5.10 | 2.10 | 0.70 | 16700 | ||
| 70 | 35.50 | 4.00 | 5.80 | 1.80 | 0.45 | 16800 | ||
| 70 | 40.50 | 4.00 | 5.60 | 1.60 | 0.40 | 16900 | ||
| 70 | 40.50 | 5.00 | 6.20 | 1.20 | 0.24 | 17000 | ||
| 71 | 36.00 | 2.00 | 4.60 | 2.60 | 1.30 | 017100C | ||
| 71 | 36.00 | 2.50 | 4.50 | 2.00 | 0.80 | 017200B | ||
| 71 | 36.00 | 4.00 | 5.60 | 1.60 | 0.40 | 017300A | ||
| 80 | 31.00 | 2.50 | 5.30 | 2.80 | 1.12 | 17400 | ||
| 80 | 31.00 | 3.00 | 5.50 | 2.50 | 0.83 | 17500 | ||
| 80 | 31.00 | 4.00 | 6.10 | 2.10 | 0.53 | 17600 | ||
| 80 | 36.00 | 3.00 | 5.70 | 2.70 | 0.90 | 17700 | ||
| 80 | 36.00 | 4.00 | 6.20 | 2.20 | 0.55 | 17800 | ||
| 80 | 41.00 | 2.25 | 5.20 | 2.95 | 1.31 | 017850C | ||
| 80 | 41.00 | 3.00 | 5.30 | 2.30 | 0.77 | 017900B | ||
| 80 | 41.00 | 4.00 | 6.20 | 2.20 | 0.55 | 18000 | ||
| 80 | 41.00 | 5.00 | 6.70 | 1.70 | 0.34 | 018100A | ||
| 90 | 46.00 | 2.50 | 5.70 | 3.20 | 1.28 | 018 200 C | ||
| 90 | 46.00 | 3.50 | 6.00 | 2.50 | 0.71 | 018 300 B | ||
| 90 | 46.00 | 5.00 | 7.00 | 2.00 | 0.40 | 018 400 A |
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | DIN2093A |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | BELLEVILLE,DISCSPRING |
| Diameter | 8,10,12.5,14,16,18,20,22.5,25,28,31.5,35.5,40,45,50,56,63,71,80,90,100,112,125,140,160,180,200,225,250 |
| Length | NON |