Schnorr Metric Conical Ribbed Locking Washer VS Medium Steel C60S

SKU: 1501
Details
Details

Schnorr safety washers type ‘VS’ can be used with high-strength bolts of the grade 8.8-10.9 without any restrictions.

This extra strong safety washer has a greater thickness for higher pre-tensioning loads. The outside inside diameter as well and the dimensions are the same as the ‘S’ type.

h max: Maximum dimension as delivered  h min: Minimum dimension after the load test  

mm NomInch nomd1d2sh minh max
53/16"5.39.00.90.951.3
6 6.410.00.90.951.4
85/16"8.413.01.11.151.7
103/8"10.516.01.41.502.0
12 13.018.01.41.552.1
14 15.022.01.41.652.2
165/8"17.024.01.92.052.6
18 19.027.01.92.152.7
20 21.030.01.92.102.8
227/8"23.033.01.92.303.0
24 25.636.02.42.703.4
25.41"38.027.02.52.953.4
27 28.639.02.42.803.5
301.1/8"31.645.02.43.053.8
361.3/8"38.054.03.03.754.5

 

 

SCHNORR Metric Conical Ribbed Locking Washer VS Medium Steel Similar DIN9250 VS 9250 sku 1501

 

 

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberDIN9250VS
Second Standard-
DriveNon
HeadNON
American Generic Brand Term SCHNORR,BELLEVILLE
Diameter 5,6,8,10,12,14,16,18,20,22,24,25.4,27,30,33,36