Metric Nord-Lock SP Large O/D Washer Delta Protekt Steel

SKU: 1503
Details
Details

Metric Nord-Lock SP Large O/D Washer Delta Protekt Steel


fastener nord-lock

 

Dd1d2h
M3.53.90009.00001.8000
M44.40009.00001.8000
M55.400010.80001.8000
M66.500013.50002.5000
M88.700016.60002.5000
M1010.700021.00002.5000
M1415.200030.70003.4000
M1617.000030.70003.4000
M1819.500034.50003.4000
M2021.400039.00003.4000
M2223.400042.00004.6000
M2425.300048.50004.6000
M2728.400048.50005.8000
M3031.400058.50006.6000
M3334.400058.50006.6000
M36  37.4000  63.0000  6.6000  

nordlock lock washer Metric Nord-Lock Paired Ribbed Locking Washer Heavy Steel threadrive

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand TermNORDLOCK
Diameter M3.5,M4,M5,M6,M8,M10,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36
LengthNON
Tags