Schnorr Metric Conical Ribbed Locking Washer VS Medium Steel C60S
Schnorr safety washers type ‘VS’ can be used with high-strength bolts of the grade 8.8-10.9 without any restrictions.
This extra strong safety washer has a greater thickness for higher pre-tensioning loads. The outside inside diameter as well and the dimensions are the same as the ‘S’ type.
h max: Maximum dimension as delivered h min: Minimum dimension after the load test
| mm Nom | Inch nom | d1 | d2 | s | h min | h max |
| 5 | 3/16" | 5.3 | 9.0 | 0.9 | 0.95 | 1.3 |
| 6 | 6.4 | 10.0 | 0.9 | 0.95 | 1.4 | |
| 8 | 5/16" | 8.4 | 13.0 | 1.1 | 1.15 | 1.7 |
| 10 | 3/8" | 10.5 | 16.0 | 1.4 | 1.50 | 2.0 |
| 12 | 13.0 | 18.0 | 1.4 | 1.55 | 2.1 | |
| 14 | 15.0 | 22.0 | 1.4 | 1.65 | 2.2 | |
| 16 | 5/8" | 17.0 | 24.0 | 1.9 | 2.05 | 2.6 |
| 18 | 19.0 | 27.0 | 1.9 | 2.15 | 2.7 | |
| 20 | 21.0 | 30.0 | 1.9 | 2.10 | 2.8 | |
| 22 | 7/8" | 23.0 | 33.0 | 1.9 | 2.30 | 3.0 |
| 24 | 25.6 | 36.0 | 2.4 | 2.70 | 3.4 | |
| 25.4 | 1" | 38.0 | 27.0 | 2.5 | 2.95 | 3.4 |
| 27 | 28.6 | 39.0 | 2.4 | 2.80 | 3.5 | |
| 30 | 1.1/8" | 31.6 | 45.0 | 2.4 | 3.05 | 3.8 |
| 36 | 1.3/8" | 38.0 | 54.0 | 3.0 | 3.75 | 4.5 |
SCHNORR Metric Conical Ribbed Locking Washer VS Medium Steel Similar DIN9250 VS 9250 sku 1501
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | DIN9250VS |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | SCHNORR,BELLEVILLE |
| Diameter | 5,6,8,10,12,14,16,18,20,22,24,25.4,27,30,33,36 |
| Length | NON |