METRICItem X2  X1  X3 BOX
3H-HLS-3          3.40          7.00          1.70200
3.5H-HLS-3.5          3.90          7.60          1.70200
4H-HLS-4          4.40          7.60          1.70200
5H-HLS-5          5.40          9.00          1.70200
6H-HLS-6          6.50        10.80          1.70200
8H-HLS-8          8.60        13.50          2.70200
10H-HLS-10        10.70        16.60          2.70200
11H-HLS-11        11.40        18.50          2.70200
12H-HLS-12        13.00        19.50          2.70200
14H-HLS-14        15.20        23.00          3.70100
16H-HLS-16        17.00        25.40          3.70100
18H-HLS-18        19.50        29.00          3.70100
20H-HLS-20        21.40        30.70          3.70100
22H-HLS-22        23.40        34.50          3.70100
24H-HLS-24        25.30        39.00          3.70100
27H-HLS-27        28.40        42.00          6.7050
30H-HLS-30        31.40        47.00          6.7050
33H-HLS-33        34.40        48.50          6.7025
36H-HLS-36        37.40        55.00          6.7025
39H-HLS-39        40.40        58.50          6.7025
42H-HLS-42        43.20        63.00          6.7025
45H-HLS-45        46.20        70.00          7.0025
48H-HLS-48        49.60        75.00          7.0025
52H-HLS-52        53.60        80.00          7.001
56H-HLS-56        59.10        85.00          7.001
60H-HLS-60        63.10        90.00          7.001
64H-HLS-64        67.10        95.00          7.001
68H-HLS-68        71.10     100.00          9.501
72H-HLS-72        75.10     105.00          9.501
76H-HLS-76        79.10     110.00          9.501

Heico-Lock® Steel Wedge Lock Washers

Heico-Lock® Steel Wedge Lock Washers are made of SAE J-403-AISI 1042/1045 or similar high carbon steel. 

Heico-Lock Steel Lock Washers

Heico-Lock® Wedge Lock Washers are perfectly suited to work with structural grade and high tensile bolts and nuts (8.8, 10.9, 12.9., ASTM 574). 

Metric Heico Lock Wedge Lock Washer Standard HLS Hardened Steel

 

 

 

 

 

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand TermHeico-lock
DiameterMetric
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.