Inch Single Coil Square Section Spring Washer Spring-Steel BS1802A
Inch Single Coil Square Section Spring Washer Spring-Steel BS1802A
| D | d max | d min | d2 max | s | swg |
|---|---|---|---|---|---|
| 1/8" | 0.1370 | 0.1290 | 0.2050 | 0.0320 | 21.0000 |
| 5/32" | 0.1700 | 0.1600 | 0.2520 | 0.0400 | 19.0000 |
| 3/16" | 0.2020 | 0.1920 | 0.3300 | 0.0640 | 16.0000 |
| 1/4" | 0.2670 | 0.2550 | 0.4250 | 0.0720 | 15.0000 |
| 5/16" | 0.3340 | 0.3200 | 0.5030 | 0.0800 | 14.0000 |
| 3/8" | 0.3990 | 0.3830 | 0.5900 | 0.0920 | 13.0000 |
| 7/16" | 0.4610 | 0.4450 | 0.6770 | 0.1040 | 12.0000 |
| 1/2" | 0.5240 | 0.5080 | 0.7630 | 0.1160 | 11.0000 |
| 9/16" | 0.5900 | 0.5700 | 0.8800 | 0.1280 | 10.0000 |
| 5/8" | 0.6600 | 0.6360 | 0.9760 | 0.1440 | 9.0000 |
| 3/4" | 0.7900 | 0.7620 | 1.1650 | 0.1760 | 7.0000 |
| 7/8" | 9.2500 | 0.8900 | 1.3600 | 0.2120 | 5.0000 |
| 1." | 1.0520 | 1.0160 | 1.5260 | 0.2320 | 4.0000 |
| 1.1/8" | 1.1840 | 1.1450 | 1.6900 | 0.2520 | 3.0000 |
Inch Single Coil Square Section Spring Washer Spring-Steel BS 1802 A s/c sq split lock washers
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | BS1802A |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | SPLITLOCK |
| Diameter | 1/8",5/32",3/16",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8" |
| Length | NON |