Inch Paired Ribbed Locking Washer USA Type Case Hardened Steel

SKU: 1521
Details
Details
Inch Paired Ribbed Locking Washer USA Type Case Hardened Steel
Dd1d2h pair
1/4"0.26200.49500.1270
5/16"0.32600.62800.1420
3/8"0.40900.70500.1600
7/16"0.45000.88000.1530
1/2"0.51000.93700.1660
9/16"0.57201.12800.1750
5/8"0.65101.24700.1880
3/4"0.82001.38100.2420
7/8"0.88301.47000.2680
1”1.01501.62600.2560
1-1/8"1.14001.71500.2560
1-1/4"1.27501.87500.2650
1-3/8"1.46902.19600.2650
1-1/2"1.52302.19600.2650
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand Term DISCLOCK,NORDLOCK
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1”,1-1/8",1-1/4",1-3/8",1-1/2"
LengthNON