Metric Load Indicating Washer DTI with Pips Hardened Steel HSFG BS EN 14399-9

SKU: 1552
Details
Details

 

Metric Load Indicating Washer DTI with Pips Hardened Steel BS EN 14399-9

 

d M16M20M22M24M27M30M36
 d1 max            16.85            21.05            23.15            25.25            28.40            31.55            37.85
d2 max            36.80            46.00            50.60            55.20            62.10            69.00            83.10
 d3 max            25.00            29.00            33.00            38.00            43.00            46.50            56.00
 h1 min              3.00              3.50              4.00              4.00              4.00              4.00              4.00
 h2 max              6.00              6.50              7.00              7.00              7.00              7.00              7.50

 

Metric Load Indicating Washer direct Tension Indicator DTI with Pips Hardened Steel HSFG BS EN 14399-9

Additional Info
Additional Info
Weight0.0000
MaterialHARDENED STEEL
Standard Number.
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter0
LengthNON
Reviews