D d1 Max d1 Min d2 Max d2 Min h Max h Min
M1.62.09001.95005.00004.70000.70000.5000
M22.64002.50006.00005.70000.90000.6000
M2.53.14003.00008.00007.64000.90000.6000
M33.68003.500010.00009.64001.20000.8000
M3.54.18004.000010.00009.64001.40001.0000
M44.88004.700012.000011.57001.40001.0000
M55.78005.500015.000014.57001.75001.2000
M66.87006.650018.800018.37001.75001.2000
M89.12008.900025.400024.48002.30001.6000
M1011.120010.850028.000027.48002.80002.0000
M1213.570013.300034.000033.38003.50002.5000
M1415.520015.250039.000038.38003.50002.5000
M1617.520017.250044.000043.38004.00003.0000
M2022.320021.800050.000049.38004.60003.5000
M2426.120025.600056.000054.80005.10004.0000
M3033.020032.400072.000070.80005.60004.5000
M3638.920038.300090.000088.60006.40005.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberB18.22M
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36