D d1 d2 h
M1011.000021.00008.0000
M1214.000024.00008.0000
M1618.000030.00008.0000
M2022.000037.00008.0000
M2426.000044.00008.0000
M2730.000050.00008.0000
M3033.000056.00008.0000
M3336.000050.00008.0000
M3639.000066.00008.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN7989
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter M10,M12,M16,M20,M24,M27,M30