Metric Hardened Washer Steel Hv30 DIN6340
SKU:
1316
Details
Details
Metric Hardened Washer Steel Hv30 DIN6340
| D | d1 | d2 | h | | | |
|---|
| M 6 | 6.4000 | 17.0000 | 3.0000 | | | |
| M 8 | 8.4000 | 23.0000 | 4.0000 | | | |
| M 10 | 10.5000 | 28.0000 | 4.0000 | | | |
| M 12 | 13.0000 | 35.0000 | 5.0000 | | | |
| M 14 | 15.0000 | 40.0000 | 5.0000 | | | * |
| M 16 | 17.0000 | 45.0000 | 6.0000 | | | |
| M 20 | 21.0000 | 50.0000 | 6.0000 | | | |
| M 24 | 25.0000 | 60.0000 | 8.0000 | | | |
| M 30 | 31.0000 | 68.0000 | 10.0000 | | | |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL HV30 |
|---|
| Standard Number | DIN6340 |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M6,M8,M10,M12,M16,?20?24,?30 |
|---|
| Length | NON |
|---|