Metric Form C Flat Washer Steel BS4320

SKU: 1296
Details
Details

Metric Form C Flat Washer Steel BS4320

Dd1d2d3
M44.300010.00000.8000
M55.300012.50001.0000
M66.400014.00001.6000
M88.400021.00001.6000
M1010.500024.00002.0000
M1213.000028.00002.5000
M1415.000030.00002.5000
M1617.000034.00003.0000
M1819.000037.00003.0000
M2021.000039.00003.0000
M2223.000044.00003.0000
M2425.000050.00004.0000
M2728.000056.00004.0000
M3031.000060.00004.0000
M3334.000066.00005.0000
M3637.000072.00005.0000
M3940.000077.00006.0000
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS4320
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter M4,M4.5,M5,M6,M7,M8,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.