| D | d1 | d2 | h |
|---|---|---|---|
| No 0 | 0.0680 | 0.2500 | 0.0250 |
| No 1 | 0.0840 | 0.2810 | 0.0320 |
| No 2 | 0.0940 | 0.3440 | 0.0320 |
| No 3 | 0.1090 | 0.4060 | 0.0400 |
| No 4 | 0.1250 | 0.4380 | 0.0400 |
| No 5 | 0.1410 | 0.5000 | 0.0400 |
| No 6 | 0.1560 | 0.5620 | 0.0400 |
| No 8 | 0.1880 | 0.6250 | 0.0630 |
| No 10 | 0.2030 | 0.7340 | 0.0630 |
| No 12 | 0.2340 | 0.8750 | 0.0630 |
| 1/4" | 0.2810 | 1.0000 | 0.0630 |
| 5/16" | 0.3440 | 1.1250 | 0.0630 |
| 3/8" | 0.4060 | 1.2500 | 0.1000 |
| 7/16" | 0.4690 | 1.4690 | 0.1000 |
| 1/2" | 0.5310 | 1.7500 | 0.1000 |
| 9/16" | 0.5940 | 2.0000 | 0.1000 |
| 5/8" | 0.6560 | 2.2500 | 0.1600 |
| 3/4" | 0.8120 | 2.5000 | 0.1600 |
| 7/8" | 0.9380 | 2.7500 | 0.1600 |
| 1" | 1.0620 | 3.0000 | 0.1600 |
| 1.1/8" | 1.1880 | 3.2500 | 0.1600 |
| 1.1/4" | 1.3120 | 3.5000 | 0.2500 |
| 1.3/8" | 1.4380 | 3.7500 | 0.2500 |
| 1.1/2" | 1.5620 | 4.0000 | 0.2500 |
| 1.5/8" | 1.7500 | 4.2500 | 0.2500 |
| 1.3/4" | 1.8750 | 4.5000 | 0.2500 |
| 1.7/8" | 2.0000 | 4.7500 | 0.2500 |
| 2" | 2.1250 | 5.0000 | 0.2500 |
| 2 .1/4 " | 2.3750 | 5.5000 | 0.3750 |
| 2 .1/2 " | 2.6250 | 6.0000 | 0.3750 |
| 2 .3/4 " | 2.8750 | 6.5000 | 0.3750 |
| 3 " | 3.1250 | 7.0000 | 0.3750 |
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel 18/8-304-A2 |
| Standard Number | B18.22.1 |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | PLAIN |
| Diameter | No0,No1,No2,No3,No4,No5,No6,No8,No10,No12,1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",1.7/8",2",2.1/4",2.1/2",2.3/4",3" |