Inch USS Wide Washer Table 1A Stainless-Steel 18/8-304-A2 B18.22.1

SKU: 1389
Details
Details
Inch USS Wide Washer Table 1A Stainless-Steel 18/8-304-A2 B18.22.1
Dd1d2h
3/16"1/4"9/16"3/64"
1/4"5/16"3/4"1/16"
5/16"3/8"7/8"5/64"
3/8"7/16"1"5/64"
7/16"1/2"1.1/4"5/64"
1/2"9/16"1.3/8"7/64"
9/16"5/8"1.1/2"7/64"
5/8"11/16"1.3/4"9/64"
3/4"13/16"2"5/32"
7/8"15/16"2.1/4"11/64"
1"1.1/16"2.1/2"11/64"
1.1/8"1.1/4"2.3/4"11/64"
1.1/4"1.3/8"3"11/64"
1.3/8"1.1/2"3.1/4"3/16"
1.1/2"1.5/8"3.1/2"3/16"
1.5/8"1.3/4"3.3/4"3/16"
1.3/4"1.7/8"4"3/16"
1.7/8"2"4.1/4"3/16"
2"2.1/8"4.1/2"3/16"
2.1/4"2.3/8"4.3/4"7/32"
2.1/2"2.5/8"5"15/64"
2.3/4"2.7/8"5.1/4"1/4"
3"3.1/8"5.1/2"9/32"
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard NumberB18.22.1
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 3/16",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",1.7/8",2",2.1/4",2.1/2",2.3/4",3"