Inch Structural Washer RC 38-45 Hardened Steel F436

SKU: 1365
Details
Details

Inch Structural Washer RC 38-45 Hardened Steel F436 

 

D           d1           d2            h min      h max    
1/2"17/32"1.1/16"0.09700.1770
5/8"11/16"1.5/16"0.12200.1770
3/4"13/16"1.15/32"0.12200.1770
7/8"15/16"1.3/4"0.13600.1770
1"1.1/8"2"0.13600.1770
1.1/8"1.1/4"2.1/4"0.13600.1770
1.1/4"1.3/8"2.1/2"0.13600.1770
1.3/8"1.1/2"2.3/4"0.13600.1770
1.1/2"1.5/8"3"0.17800.1770
1.5/8"1.3/4"3.1/4"0.17800.2800
1.3/4"1.7/8"3.3/8"0.17800.2800
1.7/8"2"3.1/2"0.17800.2800
2"2.1/8"3.3/4"0.24000.2800
2.1/4"2.3/8"4"0.24000.3400
2.1/2"2.5/8"4.1/2"0.24000.3400
2.3/4"2.7/8"5"0.24000.3400
3"3.1/8"5.1/2"0.24000.3400
3.1/4"3.3/8"6"0.24000.3400
3.1/2"3.5/8"6.1/2"0.24000.3400
3.3/4"3.7/8"7"0.24000.3400
4"4.1/8"7.1/2"0.24000.3400

 

 

Inch Structural Washer RC 38 45 Grade C  Hardened Steel F 436

Additional Info
Additional Info
Weight0.0000
MaterialHARDENED STEEL
Standard NumberF436
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/2",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",1.7/8",2",2.1/4",2.1/2",2.3/4",3",3.1/4",3.1/2",3.3/4",4"
LengthNON