Dd1d2h
No.4"1/8"5/16"21 (1/32)
No.6"5/32"3/8"18 (3/64)
No.8"3/16"7/16"18 (3/64)
3/16"7/32"1/2"18 (3/64)
No.12"1/4"9/16"1 (1/16)
1/4"9/32"5/8"16 (1/16)
5/16"11/32"11/16"16 (1/16)
3/8"13/32"13/16"16 (1/16)
7/16"15/32"59/64"16 (1/16)
1/2"17/32"1-1/16"13 (3/32)
9/16"19/32"1-3/16"13 (3/32)
5/8"21/32"1-5/16"13 (3/32)
3/4"13/16"1-1/2"10 (9/64)
7/8"15/16"1-3/4"10 (9/64)
1"1-1/16"2"10 (9/64)
1.1/8"1-3/16"2-1/4"10 (9/64)
1.1/4"1-5/16"2-1/2"9 (5/32)
1.3/8"1-7/16"2-3/4"9 (5/32)
1.1/2"1-9/16"3"9 (5/32)
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/8-304-A2
Standard NumberB18.22.1
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter No.4",No.6",No.8",3/16",No.12",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2"
LengthNON
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.