Inch Inch Washer Table 4 Light Steel BS3410

SKU: 1373
Details
Details
Inch Inch Washer Table 4 Light Steel BS3410
D d1 Max d1 Min d2 Max d2 Min h swg h
1/4"0.27000.27000.63000.620019.00000.0400
5/16"0.33000.33000.75000.750018.00000.0480
3/8"0.40000.39000.88000.870018.00000.0480
7/16"0.46000.45001.00001.000017.00000.0560
1/2"0.52000.52001.13001.120017.00000.0560
9/16"0.59000.59001.25001.240017.00000.0560
5/8"0.66000.65001.38001.370015.00000.0720
3/4"0.78000.78001.63001.620015.00000.0720
7/8"0.91000.90001.88001.870015.00000.0720
1"1.03001.03002.13002.120013.00000.0920
1.1/8"1.16001.15002.38002.360012.00000.1040
1.1/4"1.28001.28002.63002.610011.00000.1160
1.3/8"1.41001.40002.88002.860010.00000.1280
1.1/2"1.53001.53003.13003.100010.00000.1280
1.3/4"1.78001.78003.63003.600010.00000.1280
2"2.03002.03004.13004.100010.00000.1280
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2"