Inch Inch Washer Table 3 Light Stainless-Steel BS3410

SKU: 1395
Details
Details
Inch Inch Washer Table 3 Light Stainless-Steel BS3410
D d1 Max d1 Min d2 Max d2 Min h swg h
1/4"0.27000.27000.56000.560020.00000.0360
5/16"0.33000.33000.63000.620019.00000.0400
3/8"0.40000.39000.75000.750018.00000.0480
7/16"0.46000.45000.88000.870018.00000.0480
1/2"0.52000.52001.00001.000017.00000.0560
9/16"0.59000.59001.13001.120017.00000.0560
5/8"0.66000.65001.25001.240015.00000.0720
3/4"0.78000.78001.50001.490015.00000.0720
7/8"0.91000.90001.63001.620015.00000.0720
1"1.03001.03001.88001.870015.00000.0720
1.1/8"1.16001.15002.13002.120013.00000.0920
1.1/4"1.28001.28002.38002.360011.00000.1160
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4"
LengthNON