No d1 d2 h swg h
1/4"0.28000.560016.00000.0640
5/16"0.34000.630016.00000.0640
3/8"0.41000.750016.00000.0640
7/16"0.47000.880016.00000.0640
1/2"0.53001.000016.00000.0640
9/16"0.59001.130014.00000.0800
5/8"0.66001.250014.00000.0800
3/4"0.78001.500014.00000.0800
7/8"0.88001.630014.00000.0800
1"1.03001.880014.00000.0800
1-1/8"1.16002.130014.00000.0800
1-1/4"1.28002.380014.00000.0800
1-3/8"1.41002.630014.00000.0800
1-1/2"1.53002.880014.00000.0800