Inch Inch Washer Table 7 Stainless-Steel BS3410

SKU: 1400
Details
Details
Inch Inch Washer Table 7 Stainless-Steel BS3410
No d1 d2 h swg h
1/4"0.28000.630016.00000.0640
5/16"0.34000.750014.00000.0800
3/8"0.42000.880014.00000.0800
7/16"0.47001.000012.00000.1040
1/2"0.56001.130012.00000.1040
9/16"0.63001.250010.00000.1280
5/8"0.69001.380010.00000.1280
3/4"0.81001.63009.00000.1440
7/8"0.94001.88008.00000.1600
1"1.06002.13007.00000.1760
1.1/8"1.19002.38007.00000.1760
1.1/4"1.38002.63006.00000.1920
1.3/8"1.50002.88006.00000.1920
1.1/2"1.63003.13006.00000.1920
1.5/8"1.75003.38005.00000.2120
1.3/4"1.88003.63005.00000.2120
1.7/8"2.00003.88005.00000.2120
2"2.13004.13005.00000.2120
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",1.7/8",2"