Inch Inch Washer Table 5 Stainless-Steel BS3410

SKU: 1398
Details
Details
Inch Inch Washer Table 5 Stainless-Steel BS3410
Dd1 Maxd1 Mind2 Maxd2 Minh swgh
1/4"0.27000.27000.75000.750016.00000.0600
5/16"0.33000.33000.88000.870015.00000.0700
3/8"0.40000.39001.00001.000014.00000.0800
7/16"0.46000.45001.13001.120013.00000.0900
1/2"0.52000.52001.25001.240012.00000.1000
9/16"0.59000.59001.38001.370011.00000.1200
5/8"0.66000.65001.63001.620010.00000.1300
3/4"0.78000.78001.88001.87009.00000.1400
7/8"0.91000.90002.13002.12008.00000.1600
1"1.03001.03002.38002.36006.00000.1900
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1"
LengthNON