D d1 Max d1 Min d2 Max d2 Min h swg h
1/4"0.27000.27000.56000.560017.00000.0600
5/16"0.33000.33000.63000.620015.00000.0700
3/8"0.40000.39000.75000.750015.00000.0700
7/16"0.46000.45000.88000.870013.00000.0900
1/2"0.52000.52001.00001.000013.00000.0900
9/16"0.59000.59001.13001.120012.00000.1000
5/8"0.66000.65001.25001.240011.00000.1200
3/4"0.78000.78001.50001.490010.00000.1300
7/8"0.91000.90001.63001.62009.00000.1400
1"1.03001.03001.88001.87008.00000.1600
1.1/8"1.16001.15002.13002.12007.00000.1800
1.1/4"1.28001.28002.38002.36007.00000.1800
1.3/8"1.41001.40002.63002.61006.00000.1900
1.1/2"1.53001.53002.88002.86006.00000.1900
1.3/4"1.78001.78003.38003.35005.00000.2100
2"2.03002.03003.63003.60005.00000.2100
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2"
LengthNON
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.