Inch Inch Washer Table 2 BA Steel BS3410

SKU: 1369
Details
Details
Inch Inch Washer Table 2BA Steel BS3410
D d1 Max d1 Min d2 Max d2 Min h" S.W.G. h"
14BA0.04900.04400.09700.092027.00000.0160
12BA0.06100.05600.13000.125027.00000.0160
10BA0.07800.07300.17600.171027.00000.0160
9BA0.08600.08100.19700.192027.00000.0160
8BA0.99000.09400.22800.223025.00000.0200
7BA0.11100.10600.25700.252022.00000.0280
6BA0.12300.11800.28800.283020.00000.0360
5BA0.14000.13500.33500.330020.00000.0360
4BA0.15700.15200.37800.373019.00000.0400
3BA0.17700.17200.43200.427019.00000.0400
2BA0.20200.19700.50000.495018.00000.0480
1BA0.22800.22300.56500.560018.00000.0480
0BA0.25600.25100.62500.620017.00000.0560
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 14BA,12BA,10BA,9BA,8BA,7BA,6BA,5BA,4BA,3BA,2BA,1BA,0BA
LengthNON
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.