Inch Inch Washer Table 2 BA Stainless-Steel BS3410

SKU: 1393
Details
Details
Inch Inch Washer Table 2 BA Stainless-Steel BS3410
D d1 Max d1 Min d2 Max d2 Min h" S.W.G. h"
14BA0.04900.04400.09700.092027.00000.0160
12BA0.06100.05600.13000.125027.00000.0160
10BA0.07800.07300.17600.171027.00000.0160
9BA0.08600.08100.19700.192027.00000.0160
8BA0.99000.09400.22800.223025.00000.0200
7BA0.11100.10600.25700.252022.00000.0280
6BA0.12300.11800.28800.283020.00000.0360
5BA0.14000.13500.33500.330020.00000.0360
4BA0.15700.15200.37800.373019.00000.0400
3BA0.17700.17200.43200.427019.00000.0400
2BA0.20200.19700.50000.495018.00000.0480
1BA0.22800.22300.56500.560018.00000.0480
0BA0.25600.25100.62500.620017.00000.0560
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberBS3410
Second Standard-
DriveNon
HeadNON
American Generic Brand TermPLAIN
Diameter 14BA,12BA,10BA,9BA,8BA,7BA,6BA,5BA,4BA,3BA,2BA,1BA,0BA