| D | d1 Max | d1 Min | d2 Max | d2 Min | h" S.W.G. | h" |
|---|
| 8BA | 0.1000 | 0.0900 | 0.1900 | 0.1800 | 25.0000 | 0.0200 |
| 7BA | 0.1100 | 0.1100 | 0.2100 | 0.2000 | 24.0000 | 0.0200 |
| 6BA | 0.1200 | 0.1200 | 0.2300 | 0.2300 | 23.0000 | 0.0200 |
| 5BA | 0.1400 | 0.1400 | 0.2700 | 0.2600 | 23.0000 | 0.0200 |
| 4BA | 0.1600 | 0.1500 | 0.3000 | 0.3000 | 22.0000 | 0.0300 |
| 3BA | 0.1800 | 0.1700 | 0.3400 | 0.3400 | 22.0000 | 0.0300 |
| 2BA | 0.2000 | 0.2000 | 0.3900 | 0.3900 | 21.0000 | 0.0300 |
| 1BA | 0.2300 | 0.2200 | 0.4400 | 0.4400 | 20.0000 | 0.0400 |
| 0BA | 0.2600 | 0.2500 | 0.5000 | 0.5000 | 19.0000 | 0.0400 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Nylon-66 |
|---|
| Standard Number | BS3410 |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | PLAIN |
|---|
| Diameter | 8BA,6BA,4BA,3BA,2BA,1BA,0BA |
|---|
| Length | NON |
|---|