Metric Double Dished (Wave) Crinkle Washer Beryllium Copper BS4463
D | D | F nom | F max | F min | G max | G min | H max | H min |
---|
Weight | 0.0000 |
---|---|
Material | BERYLLIUM COPPER |
Standard Number | BS4463 |
Second Standard | - |
Drive | Non |
Head | NON |
American Generic Brand Term | WAVY |
Diameter | 0 |
Length | NON |