Metric Dished Washer Spring-Steel DIN137A

SKU: 1532
Details
Details
Metric Dished Washer Spring-Steel DIN137A
D d1 d2 s h
M11.10002.50000.20000.7000
M1.21.30003.00000.20000.7000
M1.41.50003.00000.25000.8000
M1.71.80004.00000.25000.9000
M1.81.90004.00000.25000.9000
M22.20004.50000.30001.0000
M2.32.50005.00000.30001.0000
M2.52.80005.50000.30001.1000
M33.20006.00000.40001.3000
M3.53.70007.00000.40001.4000
M44.30008.00000.50001.6000
M55.300010.00000.50001.8000
M66.400011.00000.50002.2000
M77.400012.00000.50002.4000
M88.400015.00000.50003.4000
M1010.500018.00000.80004.0000
Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberDIN137A
Second Standard-
DriveNon
HeadNON
American Generic Brand TermDISHED
Diameter M1,M1.2,M1.4,M1.7,M1.8,M2,M2.3,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M10