Schnorr Metric Conical Disc Springs Spring-Steel DIN2093 35.5 to 90mm

SKU: 2706
Details
Details
DeDitt'lohoho/tho’/t’Article
35.5        18.30          0.90           2.05          1.15          1.28 011850C
35.5        18.30          1.25           2.25          1.00          0.80 011900B
35.5        18.30          2.00           2.80          0.80          0.40 012000A
40        14.30          1.25           2.65          1.40          1.12 12100
40        14.30          1.50           2.75          1.25          0.83 12200
40        14.30          2.00           3.05          1.05          0.53 12300
40        16.30          1.50           2.80          1.30          0.87 12400
40        16.30          2.00           3.10          1.10          0.55 12500
40        18.30          2.00           3.15          1.15          0.58 12600
40        20.40          1.00           2.30          1.30          1.30 012700C
40        20.40          1.50           2.65          1.15          0.77 012800B
40        20.40          2.00           3.10          1.10          0.55 12900
40        20.40          2.25           3.15          0.90          0.40 013000A
40        20.40          2.50           3.45          0.95          0.38 13100
45        22.40          1.25           2.85          1.60          1.28 013250C
45        22.40          1.75           3.05          1.30          0.74 013300B
45        22.40          2.50           3.50          1.00          0.40 013400A
50        18.40          1.25           2.85          1.60          1.28 13500
50        18.40          1.50           3.30          1.80          1.20 13600
50        18.40          2.00           3.50          1.50          0.75 13700
50        18.40          2.50           4.10          1.60          0.64 13800
50        18.40          3.00           4.40          1.40          0.47 13900
50        20.40          2.00           3.50          1.50          0.75 14000
50        20.40          2.50           3.85          1.35          0.54 14100
50        22.40          2.00           3.60          1.60          0.80 14200
50        22.40          2.50           3.90          1.40          0.56 14300
50        25.40          1.25           2.85          1.60          1.28 014400C
50        25.40          1.50           3.10          1.60          1.07 14500
50        25.40          2.00           3.40          1.40          0.70 014600B
50        25.40          2.50           3.90          1.40          0.56 14700
50        25.40          3.00           4.10          1.10          0.37 014800A
56        28.50          1.50           3.45          1.95          1.30 014950C
56        28.50          2.00           3.60          1.60          0.80 015000B
56        28.50          3.00           4.30          1.30          0.43 015100A
60        20.50          2.00           4.10          2.10          1.05 15200
60        20.50          2.50           4.30          1.80          0.72 15300
60        20.50          3.00           4.70          1.70          0.57 15400
60        25.50          2.50           4.40          1.90          0.76 15500
60        25.50          3.00           4.65          1.65          0.55 15600
60        30.50          2.50           4.30          1.80          0.72 15700
60        30.50          3.00           4.70          1.70          0.57 15800
60        30.50          3.50           5.00          1.50          0.43 15900
63        31.00          1.80           4.15          2.35          1.31 016050C
63        31.00          2.50           4.25          1.75          0.70 016100B
63        31.00          3.00           4.80          1.80          0.60 16200
63        31.00          3.50           4.90          1.40          0.40 016300A
70        25.50          2.00           4.50          2.50          1.25 16400
70        30.50          2.50           4.90          2.40          0.96 16500
70        30.50          3.00           5.10          2.10          0.70 16600
70        35.50          3.00           5.10          2.10          0.70 16700
70        35.50          4.00           5.80          1.80          0.45 16800
70        40.50          4.00           5.60          1.60          0.40 16900
70        40.50          5.00           6.20          1.20          0.24 17000
71        36.00          2.00           4.60          2.60          1.30 017100C
71        36.00          2.50           4.50          2.00          0.80 017200B
71        36.00          4.00           5.60          1.60          0.40 017300A
80        31.00          2.50           5.30          2.80          1.12 17400
80        31.00          3.00           5.50          2.50          0.83 17500
80        31.00          4.00           6.10          2.10          0.53 17600
80        36.00          3.00           5.70          2.70          0.90 17700
80        36.00          4.00           6.20          2.20          0.55 17800
80        41.00          2.25           5.20          2.95          1.31 017850C
80        41.00          3.00           5.30          2.30          0.77 017900B
80        41.00          4.00           6.20          2.20          0.55 18000
80        41.00          5.00           6.70          1.70          0.34 018100A
90        46.00          2.50           5.70          3.20          1.28 018 200 C
90        46.00          3.50           6.00          2.50          0.71 018 300 B
90        46.00          5.00           7.00          2.00          0.40 018 400 A
Additional Info
Additional Info
Weight0.0000
MaterialSpring-Steel
Standard NumberDIN2093A
Second Standard-
DriveNon
HeadNON
American Generic Brand Term BELLEVILLE,DISCSPRING
Diameter 8,10,12.5,14,16,18,20,22.5,25,28,31.5,35.5,40,45,50,56,63,71,80,90,100,112,125,140,160,180,200,225,250
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.