Schnorr Metric Conical Disc Springs Spring-Steel DIN2093 Up to 34mm
| De | Di | t | t' | lo | ho | ho/t | ho’/t’ | Article |
| 6 | 3.20 | 0.30 | 0.45 | 0.15 | 0.50 | 100 | ||
| 8 | 3.20 | 0.20 | 0.40 | 0.20 | 1.00 | 200 | ||
| 8 | 3.20 | 0.30 | 0.55 | 0.25 | 0.83 | 300 | ||
| 8 | 3.20 | 0.40 | 0.60 | 0.20 | 0.50 | 400 | ||
| 8 | 4.20 | 0.20 | 0.45 | 0.25 | 1.25 | 000550C | ||
| 8 | 4.20 | 0.30 | 0.55 | 0.25 | 0.83 | 000600B | ||
| 8 | 4.20 | 0.40 | 0.60 | 0.20 | 0.50 | 000700A | ||
| 10 | 3.20 | 0.30 | 0.65 | 0.35 | 1.17 | 800 | ||
| 10 | 3.20 | 0.40 | 0.70 | 0.30 | 0.75 | 900 | ||
| 10 | 3.20 | 0.50 | 0.75 | 0.25 | 0.50 | 1000 | ||
| 10 | 4.20 | 0.40 | 0.70 | 0.30 | 0.75 | 1100 | ||
| 10 | 4.20 | 0.50 | 0.75 | 0.25 | 0.50 | 1200 | ||
| 10 | 5.20 | 0.25 | 0.55 | 0.30 | 1.20 | 001300C | ||
| 10 | 5.20 | 0.40 | 0.70 | 0.30 | 0.75 | 001400B | ||
| 10 | 5.20 | 0.50 | 0.75 | 0.25 | 0.50 | 001500A | ||
| 12 | 4.20 | 0.40 | 0.80 | 0.40 | 1.00 | 1600 | ||
| 12 | 4.20 | 0.50 | 0.85 | 0.35 | 0.70 | 1700 | ||
| 12 | 4.20 | 0.60 | 1.00 | 0.40 | 0.67 | 1800 | ||
| 12 | 5.20 | 0.50 | 0.90 | 0.40 | 0.80 | 1900 | ||
| 12 | 5.20 | 0.60 | 0.95 | 0.35 | 0.58 | 2000 | ||
| 12 | 6.20 | 0.50 | 0.85 | 0.35 | 0.70 | 2100 | ||
| 12 | 6.20 | 0.60 | 0.95 | 0.35 | 0.58 | 2200 | ||
| 12.5 | 5.20 | 0.50 | 0.85 | 0.35 | 0.70 | 2300 | ||
| 12.5 | 6.20 | 0.35 | 0.80 | 0.45 | 1.29 | 002050C | ||
| 12.5 | 6.20 | 0.50 | 0.85 | 0.35 | 0.70 | 002500B | ||
| 12.5 | 6.20 | 0.70 | 1.00 | 0.30 | 0.43 | 002700A | ||
| 14 | 7.20 | 0.35 | 0.80 | 0.45 | 1.29 | 002750C | ||
| 14 | 7.20 | 0.50 | 0.90 | 0.40 | 0.80 | 002800B | ||
| 14 | 7.20 | 0.80 | 1.10 | 0.30 | 0.38 | 002900A | ||
| 15 | 5.20 | 0.40 | 0.95 | 0.55 | 1.38 | 3000 | ||
| 15 | 5.20 | 0.50 | 1.00 | 0.50 | 1.00 | 3100 | ||
| 15 | 5.20 | 0.60 | 1.05 | 0.45 | 0.75 | 3200 | ||
| 15 | 5.20 | 0.70 | 1.10 | 0.40 | 0.57 | 3300 | ||
| 15 | 6.20 | 0.50 | 1.00 | 0.50 | 1.00 | 3500 | ||
| 15 | 6.20 | 0.60 | 1.05 | 0.45 | 0.75 | 3600 | ||
| 15 | 6.20 | 0.70 | 1.10 | 0.40 | 0.57 | 3700 | ||
| 15 | 8.20 | 0.70 | 1.10 | 0.40 | 0.57 | 3800 | ||
| 15 | 8.20 | 0.80 | 1.20 | 0.40 | 0.50 | 3900 | ||
| 16 | 8.20 | 0.40 | 0.90 | 0.50 | 1.25 | 004100C | ||
| 16 | 8.20 | 0.60 | 1.05 | 0.45 | 0.75 | 004300B | ||
| 16 | 8.20 | 0.70 | 1.15 | 0.45 | 0.64 | 4400 | ||
| 16 | 8.20 | 0.80 | 1.20 | 0.40 | 0.50 | 4500 | ||
| 16 | 8.20 | 0.90 | 1.25 | 0.35 | 0.39 | 004600A | ||
| 18 | 6.20 | 0.40 | 1.00 | 0.60 | 1.50 | 4700 | ||
| 18 | 6.20 | 0.50 | 1.10 | 0.60 | 1.20 | 4800 | ||
| 18 | 6.20 | 0.60 | 1.20 | 0.60 | 1.00 | 4900 | ||
| 18 | 6.20 | 0.70 | 1.25 | 0.55 | 0.79 | 5000 | ||
| 18 | 6.20 | 0.80 | 1.30 | 0.50 | 0.63 | 5100 | ||
| 18 | 8.20 | 0.50 | 1.10 | 0.60 | 1.20 | 5200 | ||
| 18 | 8.20 | 0.70 | 1.25 | 0.55 | 0.79 | 5300 | ||
| 18 | 8.20 | 0.80 | 1.30 | 0.50 | 0.63 | 5400 | ||
| 18 | 8.20 | 1.00 | 1.40 | 0.40 | 0.40 | 5500 | ||
| 18 | 9.20 | 0.45 | 1.05 | 0.60 | 1.33 | 005550C | ||
| 18 | 9.20 | 0.70 | 1.20 | 0.50 | 0.71 | 005600B | ||
| 18 | 9.20 | 1.00 | 1.40 | 0.40 | 0.40 | 005700A | ||
| 20 | 8.20 | 0.60 | 1.30 | 0.70 | 1.17 | 5800 | ||
| 20 | 8.20 | 0.70 | 1.35 | 0.65 | 0.93 | 5900 | ||
| 20 | 8.20 | 0.80 | 1.40 | 0.60 | 0.75 | 6000 | ||
| 20 | 8.20 | 0.90 | 1.45 | 0.55 | 0.61 | 6100 | ||
| 20 | 8.20 | 1.00 | 1.55 | 0.55 | 0.55 | 6200 | ||
| 20 | 10.20 | 0.50 | 1.15 | 0.65 | 1.30 | 006300C | ||
| 20 | 10.20 | 0.80 | 1.35 | 0.55 | 0.69 | 006400B | ||
| 20 | 10.20 | 0.90 | 1.45 | 0.55 | 0.61 | 6500 | ||
| 20 | 10.20 | 1.00 | 1.55 | 0.55 | 0.55 | 6600 | ||
| 20 | 10.20 | 1.10 | 1.55 | 0.45 | 0.41 | 006700A | ||
| 20 | 10.20 | 1.25 | 1.75 | 0.50 | 0.40 | 6800 | ||
| 20 | 10.20 | 1.50 | 1.80 | 0.30 | 0.20 | 6900 | ||
| 22.5 | 11.20 | 0.60 | 1.40 | 0.80 | 1.33 | 007000C | ||
| 22.5 | 11.20 | 0.80 | 1.45 | 0.65 | 0.81 | 007100B | ||
| 22.5 | 11.20 | 1.25 | 1.75 | 0.50 | 0.40 | 007200A | ||
| 23 | 8.20 | 0.70 | 1.50 | 0.80 | 1.14 | 7400 | ||
| 23 | 8.20 | 0.80 | 1.55 | 0.75 | 0.94 | 7500 | ||
| 23 | 8.20 | 0.90 | 1.60 | 0.70 | 0.78 | 7600 | ||
| 23 | 8.20 | 1.00 | 1.70 | 0.70 | 0.70 | 7700 | ||
| 23 | 10.20 | 0.90 | 1.65 | 0.75 | 0.83 | 7800 | ||
| 23 | 10.20 | 1.00 | 1.70 | 0.70 | 0.70 | 7900 | ||
| 23 | 10.20 | 1.25 | 1.90 | 0.65 | 0.52 | 8000 | ||
| 23 | 12.20 | 1.00 | 1.60 | 0.60 | 0.60 | 8100 | ||
| 23 | 12.20 | 1.25 | 1.85 | 0.60 | 0.48 | 8200 | ||
| 23 | 12.20 | 1.50 | 2.00 | 0.50 | 0.33 | 8350 | ||
| 25 | 10.20 | 1.00 | 1.75 | 0.75 | 0.75 | 8600 | ||
| 25 | 12.20 | 0.70 | 1.60 | 0.90 | 1.29 | 008700C | ||
| 25 | 12.20 | 0.90 | 1.60 | 0.70 | 0.78 | 008800B | ||
| 25 | 12.20 | 1.00 | 1.80 | 0.80 | 0.80 | 8900 | ||
| 25 | 12.20 | 1.25 | 1.95 | 0.70 | 0.56 | 9000 | ||
| 25 | 12.20 | 1.50 | 2.05 | 0.55 | 0.37 | 009100A | ||
| 28 | 10.20 | 0.80 | 1.75 | 0.95 | 1.19 | 9200 | ||
| 28 | 10.20 | 1.00 | 1.90 | 0.90 | 0.90 | 9300 | ||
| 28 | 10.20 | 1.25 | 2.05 | 0.80 | 0.64 | 9400 | ||
| 28 | 10.20 | 1.50 | 2.20 | 0.70 | 0.47 | 9500 | ||
| 28 | 12.20 | 1.00 | 1.95 | 0.95 | 0.95 | 9600 | ||
| 28 | 12.20 | 1.25 | 2.10 | 0.85 | 0.68 | 9700 | ||
| 28 | 12.20 | 1.50 | 2.25 | 0.75 | 0.50 | 9800 | ||
| 28 | 14.20 | 0.80 | 1.80 | 1.00 | 1.25 | 009900C | ||
| 28 | 14.20 | 1.00 | 1.80 | 0.80 | 0.80 | 010000B | ||
| 28 | 14.20 | 1.25 | 2.10 | 0.85 | 0.68 | 10100 | ||
| 28 | 14.20 | 1.50 | 2.15 | 0.65 | 0.43 | 010200A | ||
| 31.5 | 12.20 | 1.00 | 2.10 | 1.10 | 1.10 | 10300 | ||
| 31.5 | 12.20 | 1.25 | 2.20 | 0.95 | 0.76 | 10400 | ||
| 31.5 | 12.20 | 1.50 | 2.35 | 0.85 | 0.57 | 10500 | ||
| 31.5 | 16.30 | 0.80 | 1.85 | 1.05 | 1.31 | 010650C | ||
| 31.5 | 16.30 | 1.25 | 2.15 | 0.90 | 0.72 | 010700B | ||
| 31.5 | 16.30 | 1.50 | 2.40 | 0.90 | 0.60 | 10800 | ||
| 31.5 | 16.30 | 1.75 | 2.45 | 0.70 | 0.40 | 010900A | ||
| 31.5 | 16.30 | 2.00 | 2.75 | 0.75 | 0.38 | 11000 | ||
| 34 | 12.30 | 1.00 | 2.25 | 1.25 | 1.25 | 11100 | ||
| 34 | 12.30 | 1.25 | 2.35 | 1.10 | 0.88 | 11200 | ||
| 34 | 12.30 | 1.50 | 2.50 | 1.00 | 0.67 | 11300 | ||
| 34 | 14.30 | 1.25 | 2.40 | 1.15 | 0.92 | 11400 | ||
| 34 | 14.30 | 1.50 | 2.55 | 1.05 | 0.70 | 11500 | ||
| 34 | 16.30 | 1.50 | 2.55 | 1.05 | 0.70 | 11600 | ||
| 34 | 16.30 | 2.00 | 2.85 | 0.85 | 0.43 | 11700 | ||
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | DIN2093A |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | BELLEVILLE,DISCSPRING |
| Diameter | 8,10,12.5,14,16,18,20,22.5,25,28,31.5,35.5,40,45,50,56,63,71,80,90,100,112,125,140,160,180,200,225,250 |
| Length | NON |