| De | Di | t | t' | lo | ho | ho/t | ho’/t’ | Article |
| 100 | 41.00 | 4.00 | 7.20 | 3.20 | 0.80 | 018 500 | ||
| 100 | 41.00 | 5.00 | 7.75 | 2.75 | 0.55 | 018 600 | ||
| 100 | 51.00 | 2.70 | 6.20 | 3.50 | 1.30 | 018 750 C | ||
| 100 | 51.00 | 3.50 | 6.30 | 2.80 | 0.80 | 018 800 B | ||
| 100 | 51.00 | 4.00 | 7.00 | 3.00 | 0.75 | 018 900 | ||
| 100 | 51.00 | 5.00 | 7.80 | 2.80 | 0.56 | 019 000 | ||
| 100 | 51.00 | 6.00 | 8.20 | 2.20 | 0.37 | 019 150 A | ||
| 112 | 57.00 | 3.00 | 6.90 | 3.90 | 1.30 | 019 250 C | ||
| 112 | 57.00 | 4.00 | 7.20 | 3.20 | 0.80 | 019 300 B | ||
| 112 | 57.00 | 6.00 | 8.50 | 2.50 | 0.42 | 019 450 A | ||
| 125 | 41.00 | 4.00 | 8.20 | 4.20 | 1.05 | 019 500 | ||
| 125 | 51.00 | 4.00 | 8.50 | 4.50 | 1.13 | 019 600 | ||
| 125 | 51.00 | 5.00 | 8.90 | 3.90 | 0.78 | 019 700 | ||
| 125 | 51.00 | 6.00 | 9.40 | 3.40 | 0.57 | 019 850 | ||
| 125 | 61.00 | 5.00 | 9.00 | 4.00 | 0.80 | 019 900 | ||
| 125 | 61.00 | 6.00 | 9.60 | 3.60 | 0.60 | 020 050 | ||
| 125 | 61.00 | 8.00 | 7.50 | 10.90 | 2.90 | 0.45 | 020 100 | |
| 125 | 64.00 | 3.50 | 8.00 | 4.50 | 1.29 | 020 200 C | ||
| 125 | 64.00 | 5.00 | 8.50 | 3.50 | 0.70 | 020 300 B | ||
| 125 | 64.00 | 8.00 | 7.50 | 10.60 | 2.60 | 0.41 | 020 400 A | |
| 125 | 71.00 | 6.00 | 9.30 | 3.30 | 0.55 | 020 550 | ||
| 125 | 71.00 | 8.00 | 7.40 | 10.40 | 2.40 | 0.41 | 020 600 | |
| 125 | 71.00 | 10.00 | 9.20 | 11.80 | 1.80 | 0.28 | 020 700 | |
| 140 | 72.00 | 3.80 | 8.70 | 4.90 | 1.29 | 020 850 C | ||
| 140 | 72.00 | 5.00 | 9.00 | 4.00 | 0.80 | 020 900 B | ||
| 140 | 72.00 | 8.00 | 7.50 | 11.20 | 3.20 | 0.49 | 021 000 A | |
| 150 | 61.00 | 5.00 | 10.30 | 5.30 | 1.06 | 021 100 | ||
| 150 | 61.00 | 6.00 | 10.80 | 4.80 | 0.80 | 021 250 | ||
| 150 | 71.00 | 6.00 | 10.80 | 4.80 | 0.80 | 021 350 | ||
| 150 | 71.00 | 8.00 | 7.50 | 12.00 | 4.00 | 0.60 | 021 400 | |
| 150 | 81.00 | 8.00 | 7.50 | 11.70 | 3.70 | 0.56 | 021 500 | |
| 150 | 81.00 | 10.00 | 9.30 | 13.00 | 3.00 | 0.40 | 021 600 | |
| 160 | 82.00 | 4.30 | 9.90 | 5.60 | 1.30 | 021650C | ||
| 160 | 82.00 | 6.00 | 10.50 | 4.50 | 0.75 | 021750B | ||
| 160 | 82.00 | 10.00 | 9.40 | 13.50 | 3.50 | 0.44 | 021800A | |
| 180 | 92.00 | 4.80 | 11.00 | 6.20 | 1.29 | 021850C | ||
| 180 | 92.00 | 6.00 | 11.10 | 5.10 | 0.85 | 021950B | ||
| 180 | 92.00 | 10.00 | 9.40 | 14.00 | 4.00 | 0.49 | 022000A | |
| 200 | 82.00 | 8.00 | 7.60 | 14.20 | 6.20 | 0.87 | 22100 | |
| 200 | 82.00 | 10.00 | 9.60 | 15.50 | 5.50 | 0.61 | 22200 | |
| 200 | 82.00 | 12.00 | 11.50 | 16.60 | 4.60 | 0.44 | 22300 | |
| 200 | 92.00 | 10.00 | 9.50 | 15.60 | 5.60 | 0.64 | 22400 | |
| 200 | 92.00 | 12.00 | 11.40 | 16.80 | 4.80 | 0.47 | 22500 | |
| 200 | 92.00 | 14.00 | 13.10 | 18.10 | 4.10 | 0.38 | 22600 | |
| 200 | 102.00 | 5.50 | 12.50 | 7.00 | 1.27 | 022650C | ||
| 200 | 102.00 | 8.00 | 7.50 | 13.60 | 5.60 | 0.81 | 022700B | |
| 200 | 102.00 | 10.00 | 9.40 | 15.60 | 5.60 | 0.66 | 22800 | |
| 200 | 102.00 | 12.00 | 11.25 | 16.20 | 4.20 | 0.44 | 022900A | |
| 200 | 102.00 | 14.00 | 13.10 | 18.20 | 4.20 | 0.39 | 23000 | |
| 200 | 112.00 | 12.00 | 11.10 | 16.20 | 4.20 | 0.46 | 23100 | |
| 200 | 112.00 | 14.00 | 12.90 | 17.50 | 3.50 | 0.36 | 23200 | |
| 200 | 112.00 | 16.00 | 14.80 | 18.80 | 2.80 | 0.27 | 23300 | |
| 225 | 112.00 | 6.50 | 6.20 | 13.60 | 7.10 | 1.19 | 023350C | |
| 225 | 112.00 | 8.00 | 7.50 | 14.50 | 6.50 | 0.93 | 023400B | |
| 225 | 112.00 | 12.00 | 11.25 | 17.00 | 5.00 | 0.51 | 023500A | |
| 250 | 102.00 | 10.00 | 9.60 | 18.00 | 8.00 | 0.88 | 23600 | |
| 250 | 102.00 | 12.00 | 11.50 | 19.00 | 7.00 | 0.65 | 23700 | |
| 250 | 127.00 | 7.00 | 6.70 | 14.80 | 7.80 | 1.21 | 023750C | |
| 250 | 127.00 | 10.00 | 9.40 | 17.00 | 7.00 | 0.81 | 023800B | |
| 250 | 127.00 | 12.00 | 11.25 | 19.30 | 7.30 | 0.72 | 23900 | |
| 250 | 127.00 | 14.00 | 13.10 | 19.60 | 5.60 | 0.50 | 024000A | |
| 250 | 127.00 | 16.00 | 15.00 | 21.80 | 5.80 | 0.45 | 24100 |
| Weight | 0.0000 |
|---|---|
| Material | Spring-Steel |
| Standard Number | DIN2093A |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | BELLEVILLE,DISCSPRING |
| Diameter | 8,10,12.5,14,16,18,20,22.5,25,28,31.5,35.5,40,45,50,56,63,71,80,90,100,112,125,140,160,180,200,225,250 |
| Length | NON |