Inch Allthread ACME Stainless-Steel-A2 B1.5
Inch Allthread ACME Stainless-Steel-A2 B1.5
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel-A2 |
| Standard Number | B1.5 |
| Second Standard | - |
| Drive | Non |
| Head | NON |
| American Generic Brand Term | THREADEDBAR,STUDDING |
| Diameter | TR10,TR12,TR14,TR16,TR18,TR20,TR22,TR24,TR26,TR28,TR30,TR32,TR36,TR40,TR44,TR50,TR60 |
| Length | VARIOUS |