ddd1 mind2e minkk1k2S
M512.0010.005.508.844.502.171.008.00
M614.0011.806.6011.105.202.271.1010.00
M818.0015.209.0014.497.202.701.3013.00
M1021.0017.2011.0016.649.003.241.6015.00
M1225.0020.6014.0019.0111.004.001.9017.00
M1428.0022.8016.0021.2312.504.502.2019.00
M1632.0025.7018.0024.6216.006.383.8022.00
M2039.0031.2022.0030.1418.006.493.1027.00

 

 

The Durlok® self-locking system is the solution to one of the most persistent problems in the field of fastener technology.

VIBRATION.

Durlok nuts and bolts will not loosen or unscrew even under the most severe transverse jarring and vibration.

The Durlok fastener system is effective on a wide variety of engineering materials including steel -- both heat-treated and non heat-treated, cast irons including nodular types, non-ferrous metals and sheet materials.

Durlok nuts and bolts are suitable for re-use because the serrations cause relatively little damage to the clamped material.

 

Metric Coarse Durlok Hexagon Flange Bolt Serrated Underhead Grade-12.9

Metric Coarse Durlok durlock derlock Hexagon Flange Bolt Serrated Underhead Grade-12.9

Additional Info
Additional Info
Weight0.0000
MaterialGrade-12.9
Standard Number.
Second StandardDURLOK
DriveHexagon
HeadFlange
American Generic Brand TermDURLOK
Diameter0
Length0
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.