UNC External Torx Bolt with Flange Stainless-Steel 18/10-316-A4 B18.2.1

SKU: 1845
Details
Details
UNC External Torx Bolt with Flange Stainless-Steel 18/10-316-A4 B18.2.1
Ddkk maxk mindc maxdc minh maxh mindrive
1/4”0.28700.25500.24500.37500.36500.07000.0600E8
5/16”0.36200.32300.31300.46900.4570 0..10.0900E10
3/8”0.43100.39400.38400.56200.55000.12500.1150E12
7/16”0.49900.47200.46200.65600.64200.15500.1450E14
1/2”0.57100.51500.50500.75000.73500.16000.1500E16
9/16”0.64500.55100.54100.84400.82800.16500.1530E18
5/8”0.71500.63000.62000.93800.92100.20000.1880E20
3/4”0.86000.78700.77701.12501.10700.25500.2430E24
7/8”1.00000.86600.85601.31201.29300.27000.2600E28
1”1.13801.06301.05301.50001.47900.35500.3430E32
1.1/8"1.28001.18101.17101.68801.66500.38200.3700E36
1.1/4"1.42001.29901.28901.87501.85200.42200.4100E40
1.3/8"1.56201.41701.40702.06202.03800.45300.4410E44
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel 18/10-316-A4
Standard NumberB18.2.1
Second Standard-
DriveTorx,hexalobular,socket
HeadFlange
American Generic Brand Term6LOBE
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8"
Length1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8