Metric Coarse External Torx Bolt with Flange Grade-10.9 DIN34800

SKU: 1819
Details
Details
Metric Coarse External Torx Bolt with Flange Grade-10.9 DIN34800
Dbds maxds mindkk maxk min
M435.00004.00003.82004.60004.50004.2500
M540.00005.00004.82005.55005.50005.2500
M650.00006.00005.82007.30006.50006.2500
M865.00008.00007.78009.20008.20007.9500
M1080.000010.00009.780010.950010.00009.7500
M1280.000012.000011.730012.650012.000011.7500
M1480.000014.000013.730016.400014.000013.7500
M1680.000016.000015.730018.150016.000015.7500
M1880.000018.000017.730021.850018.000017.7500
M2080.000020.000019.670021.850020.000019.7500
Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberDIN34800
Second Standard-
DriveTorx,hexalobular,socket
HeadFlange
American Generic Brand Term6LOBE
Diameter M4,M5,M6,M7,M8,M10,M12,M14,M16,M18,M20
Length16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100