Metric Torx Countersunk Head Self Tapping Screw AB Case Hardened Steel DIN7982

SKU: 1836
Details
Details
Metric Torx Countersunk Head Self Tapping Screw AB Case Hardened Steel DIN7982
DDF nomF maxF minG maxG minH maxH min
Additional Info
Additional Info
Weight0.0000
MaterialCASE HARDENED STEEL
Standard NumberDIN7982
Second StandardISO14586
DriveTorx,hexalobular,socket
HeadCOUNTERSUNK
American Generic Brand TermFLAT,TORX
Diameter0
Length0
Reviews
Tags
Tags