UNC Splined Socket Button Head Screw Grade-12.9 B18.3

SKU: 1807
Details
Details
UNC Splined Socket Button Head Screw Grade-12.9 B18.3
dda maxa minh maxh minsm nomy minf maxf min
No.00.06000.11400.10400.03200.02600.01000.04800.02000.01000.0050
No.10.07300.13900.12900.03900.03300.01000.06000.02800.01000.0050
No.20.08600.16400.15400.04600.03800.01000.06000.02800.01000.0050
No.30.09900.18800.17600.05200.04400.01000.07200.03500.01000.0050
No.40.11200.21300.20100.05900.05100.01500.07200.03500.01000.0050
No.50.12500.23800.22600.06600.05800.01500.09600.04400.01000.0050
No.60.13800.26200.25000.07300.06300.01500.09600.04400.01000.0050
No.80.16400.31200.29800.08700.07700.01500.11100.05200.01500.0100
No.100.19000.36100.34700.10100.09100.02000.14500.07000.01500.0100
1/4"0.25000.43700.41900.13200.12200.03100.18300.08700.02000.0150
5/16"0.31250.54700.52700.16600.15200.03100.21600.10500.02000.0150
3/8"0.37500.65600.63600.19900.18500.03100.25100.12200.02000.0150
1/2"0.50000.87500.85100.26500.24500.04600.37200.17500.03000.0200
5/8"0.62501.00000.97000.33100.31100.06200.45400.21000.03000.0200
Additional Info
Additional Info
Weight0.0000
MaterialGrade-12.9
Standard NumberB18.3
Second Standard-
DriveSpline
HeadButtoncap
American Generic Brand Term-
Diameter No.0,No.1,No.2,No.3,No.4,No.5,No.6,No.8,No.10,1/4",5/16",3/8",1/2",5/8"
Length1/8"3/16",1/4",5/16",3/8",1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5."